Posted 12/31/2012 00:07 (#2787233 - in reply to #2786949) Subject: Re: Mixing 10-34-0 and 28%
west Nebraska northeast Colorado
I have had problems with the mixture forming a "slime" on the pre-orifice screens in my system. Eliminated the problem by first diluting the 10-34-0 with water.