NE Iowa | I've read the patent for Bioforge and it gives details on what it is and how it's made. You dissolve dry urea in formic acid. Then let it sit for 10 days or so and it resolidifies. Then add water to this and make it a solution again. Pottassium hydroxide (lye) is then added to balance the pH. It takes a little time but not hard to make. Costs about $1.50 or so an acre to make yourself which is about 10% of what they charge. Not sure that it does what is claims though. Used it several year but never any good side-by-sides. Now someone that sells this stuff will probably claim there is more to making it then that. But MSDS sheets and patents don't lie. Can give exact recipe if you like. | |
|